Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.830 g/cc @Temperature 316 °C |
0.0300 lb/in³ @Temperature 600 °F |
|
Duratherm S Silicone Heat Transfer Fluid Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s.. |