Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.815 g/cc @Temperature 23.9 °C |
0.0294 lb/in³ @Temperature 75.0 °F |
|
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |
|||
Density | 0.815 g/cc @Temperature -45.6 °C |
0.0294 lb/in³ @Temperature -50.0 °F |
|
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam .. |
|||
Density | 0.815 g/cc @Temperature 37.8 °C |
0.0295 lb/in³ @Temperature 100 °F |
|
Duratherm LT Paraffinic Heat Transfer Fluid Duratherm LT - heat transfer fluid engineered for applications requiring process temperatures ranging from -30°F to 600°F. Ideal for batch processing requiring heating and cooling cycles. Eliminat.. |