Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.755 g/cc @Temperature 23.9 °C |
0.0273 lb/in³ @Temperature 75.0 °F |
|
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam .. |