Polymer Property : Density = 0.275 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 7.60 g/cc

@Temperature 600 °C
0.275 lb/in³

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel
A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re..
Density 7.60 g/cc

@Temperature 600 °C
0.275 lb/in³

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel
W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E..
Density 7.60 g/cc

@Temperature 800 °C
0.275 lb/in³

@Temperature 1470 °F
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat..