Physical Properties Metric English Comments
Density 1.95 g/cc

@Temperature -54.0 °C
0.0704 lb/in³

@Temperature -65.2 °F
Solvay Specialty Polymers Galden® D02 PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Density 1.95 g/cc

@Temperature -54.0 °C
0.0704 lb/in³

@Temperature -65.2 °F
Solvay Specialty Polymers Galden® D02TS PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..