Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.063 g/cc @Temperature 35.0 °C |
0.03840 lb/in³ @Temperature 95.0 °F |
|
BASF Pluracol® 1168 Rigid Polyol Description: Pluracol® 1168 Polyol is a general purpose aromatic initiator-based polyol for rigid foams for use in a variety of applications. It is attractively priced for consideration for foaming.. |