Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.015 - 1.018 g/cc @Temperature 20.0 °C |
0.03667 - 0.03678 lb/in³ @Temperature 68.0 °F |
Highest Class, First Class |
Kazanorgsintez Monoethanolamine Production Method: Interaction of ammonia or its water solution with ethylene oxide. Application: Used in the gas and petroleum industry for absorption of acid gases and sulfur-containing organic co.. |
|||
Density | 1.015 - 1.025 g/cc @Temperature 20.0 °C |
0.03667 - 0.03703 lb/in³ @Temperature 68.0 °F |
Second Class |
Kazanorgsintez Monoethanolamine Production Method: Interaction of ammonia or its water solution with ethylene oxide. Application: Used in the gas and petroleum industry for absorption of acid gases and sulfur-containing organic co.. |
|||
Density | 1.015 - 1.05 g/cc @Temperature 20.0 °C |
0.03667 - 0.0379 lb/in³ @Temperature 68.0 °F |
Third Class |
Kazanorgsintez Monoethanolamine Production Method: Interaction of ammonia or its water solution with ethylene oxide. Application: Used in the gas and petroleum industry for absorption of acid gases and sulfur-containing organic co.. |