Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.843 g/cc @Temperature 37.8 °C |
0.0304 lb/in³ @Temperature 100 °F |
|
Duratherm FG Paraffinic Heat Transfer Fluid Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac.. |
|||
Density | 0.841 g/cc @Temperature 288 °C |
0.0304 lb/in³ @Temperature 550 °F |
|
Duratherm S Silicone Heat Transfer Fluid Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s.. |