Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.673 g/cc @Temperature 316 °C |
0.0243 lb/in³ @Temperature 600 °F |
|
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he.. |