Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 9.0 g/l | 9.0 g/l | |
Parker Chomerics Tecknit® 0002 Highly Conductive Adhesive-Sealant Silver Silicone Description: TECKNIT® 0002 is a pure silver filled, one component RTV silicone adhesive-sealant. It is ready to use without mixing and cures quickly at room temperature on exposure to moisture in .. |