Polymer Property : Volatile Organic Compounds (VOC) Content = 861 g/l
Polymer Property :
Volatile Organic Compounds (VOC) Content =
861 g/l
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Volatile Organic Compounds (VOC) Content
861
g/l
861
g/l
Dow Corning 1205 RTV PRIME COAT
Clear, film forming primer for use with all silicone RTVsInformation provided by Dow Corning