Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volatile Organic Compounds (VOC) Content = 840 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 144 - 840 g/l
144 - 840 g/l
Average value: 527 g/l Grade Count:32
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Copyright © lookpolymers.com All Rights Reserved