Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 824 g/l | 824 g/l | ASTM D3960-87 |
Lord Adhesives Aeroglaze® 9953 Epoxy Primer Thinner Aeroglaze® 9953 thinner is used to reduce Aeroglaze epoxy viscosity for spray applicationsAll information provided by Lord. |