Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 8.8 g/l | 8.8 g/l | |
Tra-Con Tra-Bond 526M04 Color Keyed High Temperature Epoxy Adhesive TRA-BOND 526M04 is a low viscosity, high-temperature, two-part epoxy formulation with a long working life. TRA-BOND 526M04 exhibits excellent wicking, and develops strong, tough mechanically stable .. |