Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 76 g/l | 76 g/l | |
Dow Corning 1200 OS PRIMER CLEAR Adhesion to metals, ceramics, rubbers, PVC's, polyesters, PET, acrylics, PUInformation provided by Dow Corning |