Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 75 g/l
75 g/l
Parker Chomerics CHO-SHIELD® 2054 Conductive Coating
CHO-SHIELD® 2054 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo..