Polymer Property : Volatile Organic Compounds (VOC) Content = 693 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 693 g/l
693 g/l
3M P595 Teak & Glass Primer
3M™ Adhesion Promoter AP596 and 3M™ Primers P590, P591, P592, P595 and P597 are low viscosity adhesion promoters recommended for use with the 3M™ 500-Series Polyurethane Adhesives/Sealants and 3M..