Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 618 g/l
618 g/l
ASTM D3960-89
Lord Adhesives Aeroglaze® Z302 Absorptive Polyurethane
Aeroglaze® Z302 absorptive polyurethane is primarily for application to substrates used in space operations. These operations include those where coatings must exhibit low outgassing characterist..