Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 599 g/l
599 g/l
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone
Volatile Organic Compounds (VOC) Content 599 g/l
599 g/l
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone