Volatile Organic Compounds (VOC) Content 596 g/l
596 g/l
USEPA Method 24
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Volatile Organic Compounds (VOC) Content 596 g/l
596 g/l
USEPA Method 24
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..