Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 582 g/l | 582 g/l | |
3M Scotch-Weld™ 78 ET Polystyrene Foam Insulation Cylinder Spray Adhesive A tacky industrial grade spray adhesive with a long open time designed for bonding polystyrene and other insulation materials to a variety of surfacesFeatures:It can permanently bond polystyrene foa.. |