Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 563 g/l | 563 g/l | |
Aremco Lamp-Coat™ LC4010-BT High Temperature Coating, Silicone Aluminum-filled coating for application over black top coated headlamps to 1020 °F (550 °C). |
|||
Volatile Organic Compounds (VOC) Content | 563 g/l | 563 g/l | |
3M Scotch-Weld™ Foam Fast 74 Cylinder Spray Adhesive An extremely fast tacking industrial grade spry adhesive for bonding foam and fabricFeatures:Used for bonding flexible urethane or latex foam together and to other materials such as wood, metal and .. |