Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 544 g/l | 544 g/l | |
3M Scotch-Weld™ HoldFast 70 Cylinder Spray Adhesive Extremely versatile, fast tracking industrial grade spray adhesive with unique wide-web spray pattern. Ideal for bonding a variety of substrates, including polystyrene.Features: Creates quick perman.. |