Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 505 g/l
505 g/l
3M Scotch-Weld™ 78 HT Hi-Temperature Polystyrene Foam Insulation Spray Adhesive (Bulk)
A high strength, high temperature resistant, industrial grade spray adhesive with a long open time designed for bonding most types of insulation such as fiberglass, expanded polystyrene foam, and ex..