Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | <= 50 g/l | <= 50 g/l | |
Dow Corning 777 WATER REPELLENT Dow Corning® 777 Water Repellent is a water-dilutable solution of potassium methyl siliconate designed to impart water repellency to a wide variety of surfaces. Supplied at a concentration of 40 pe.. |