Polymer Property : Volatile Organic Compounds (VOC) Content = 485 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 425 - 485 g/l
425 - 485 g/l
depending on color
3M Scotchkote™ UV 840 Urethane Coating
Scotchkote Urethane Coating UV 840 has been developed to provide a durable gloss finish for use as the final coat of 3M coating systems in the construction and transport industries, where an ease of..