Polymer Property : Volatile Organic Compounds (VOC) Content = 361 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 361 g/l
361 g/l
Parker Chomerics CHO-BOND 4669 Conductive Caulk/Sealant
Chomerics two-component conductive epoxy caulks provide excellent adhesion to dissimilar substrates and can be used in lap or butt joint applications. They feature large silver-plated-copper particl..