Polymer Property : Volatile Organic Compounds (VOC) Content = 36 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 36 g/l
36 g/l
Blue River Coatings Hydro-Gloss 2-Part Polyurethane Top Coat
BLUE RIVER COATINGS HYDRO-GLOSS 2-PART POLYURETHANE TOPCOAT is a water dispersible polyisocyanate coating. HYDRO-GLOSS provides outstanding coverage, excellent durability, and ease of application as..