Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 359.5 g/l | 359.5 g/l | |
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h.. |