Polymer Property : Volatile Organic Compounds (VOC) Content = 355 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 355 g/l
355 g/l
9929B; ASTM D3960-89
Lord Adhesives Aeroglaze® 9929 Epoxy Primer
Aeroglaze® 9929 epoxy primer is designed to be used on properly prepared aluminum and steel surfaces for applications that require protection against corrosion.All information provided by Lord.