Polymer Property : Volatile Organic Compounds (VOC) Content = 342.7 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 342.7 g/l
342.7 g/l
Aremco Corr-Paint™ CP2000 High Temperature Protective Coating Urethane, Carbon Filled
These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h..