Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 31.2 g/l | 31.2 g/l | |
Tra-Con Tra-Bond 2111 Rigid Epoxy Staking Compound TRA-BOND 2111 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |