Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 257.6 g/l | 257.6 g/l | EPA method #24 |
Abatron Abokote 8106-1 Water-Based Epoxy Coating for Floors Abokote 8106-1 is a water-based epoxy coating that is part of the Abokote 8106-1 Flooring System which consists of this water-based epoxy coating, vinyl color chips, and Abokote 57-1 clear acrylic t.. |
|||
Volatile Organic Compounds (VOC) Content | 257.6 g/l | 257.6 g/l | EPA method #24 |
Abatron Water Epoxy Floor Coating System The Water Epoxy Floor Coating System combines beauty, durability, slip resistance, ease of application, and water resistance. Its other features and benefits include low odor on installation, easy m.. |