Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 257 g/l | 257 g/l | |
Parker Chomerics Tecknit® 0036 Two Part Flexible Adhesive-Sealant Silver-Glass Silicone Description: TECKNIT 0036 is an electrically conductive, medium viscosity, RTV silicone adhesive-sealant. This silver-plated glass filled system is formulated with a special conductive material pro.. |