Polymer Property : Volatile Organic Compounds (VOC) Content = 220 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 220 g/l
220 g/l
EPA method #24
Abatron AboCoat 8508-1 Heavy-Duty Epoxy Paint
AboCoat 8508-1 is a heavy-duty epoxy paint. It excels as a protective and decorative coating for concrete, metal, wood, and composite surfaces, indoors and outdoors. It is applied to floors, walls, ..