Polymer Property : Volatile Organic Compounds (VOC) Content = 2.74 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 2.74 g/l
2.74 g/l
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System
TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul..