Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 151 g/l
151 g/l
Parker Chomerics CHO-BOND 1030 Conductive Silicone Gasket Adhesive
Electrically conductive one-component silicone-based RTV adhesive which greatly simplifies the problem of bonding conductive silicone EMI gaskets to metal substrates. This adhesive cures on exposure..
Volatile Organic Compounds (VOC) Content 151 g/l
151 g/l
Parker Chomerics CHO-BOND 1035 Electrically Conductive Sealant
Electrically conductive, one component RTV silicone which provides both environmental sealing and EMI/RFI shielding. This sealant, filled with silver-plated glass particles, contains no acetic acid,..