Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 12.5 g/l | 12.5 g/l | |
Dow Corning TM-1951 EMULSION Dow Corning® TM-1950 Emulsion and Dow Corning® TM-1951 Emulsion are water-based silicone products with excellent dilution stability, which provide release of tissue paper from felt, fabric and wir.. |