Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 0.19 g/l | 0.19 g/l | |
Tra-Con Tra-Bond 716C01 Medium Viscosity Epoxy Adhesive TRA-BOND 716C01 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications. This two-part amber adhesive is easily mixed, used and cured at room temperature.. |