Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 40.0 - 90.0 °C | 104 - 194 °F | |
Aremco Aremco-Seal™ 613 High Temperature Glass Coating Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1150 ºF (620 ºC) |
|||
Storage Temperature | 40.0 - 90.0 °C | 104 - 194 °F | |
Aremco Aremco-Seal™ 617 High Temperature Glass Coating Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 ºF (816 ºC). |