Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | <= 35.0 °C | <= 95.0 °F | |
Protective Coating PC-Concrete™ Epoxy Concrete Anchoring and Repair System PC Concrete™ epoxy gel is an anchoring and concrete repair product. PC Concrete™ is formulated for anchoring threaded rods, bolts, rebar dowels and smooth dowels into concrete, grout filled block,.. |
|||
Storage Temperature | <= 35.0 °C | <= 95.0 °F | |
Dow Corning SYL-OFF® SB 7458 COATING Base polymer component for Syl-Off® brand solvent-based, platinum-catalyzed silicone release coatingsInformation provided by Dow Corning |
|||
Storage Temperature | <= 35.0 °C | <= 95.0 °F | |
Dow Corning SYL-OFF® SL 7688 RELEASE COATING Base polymer component for Syl-Off® solvent-based platinum catalyzed silicone release coatingsInformation provided by Dow Corning |