Polymer Property : Relative Viscosity = 50 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 45 - 50 cP
45 - 50 cP
ASTM D2857
Network Polymers Nylon 6001 L
Description: General Purpose Black NylonInformation provided by Network Polymers Inc.
Relative Viscosity 44 - 50 cP
44 - 50 cP
ASTM D789
Ascend Performance Materials Vydyne® 85XFS Nylon 66/6, General Purpose
Vydyne® 85XFS is a general-purpose PA66/6 resin. It is available in natural and is designed for extrusion-compounding applications. This copolymer PA66/6 resin provides a lower melting point and ca..