Physical Properties Metric English Comments
Relative Viscosity 45 - 49 cP
45 - 49 cP
Formic Acid; ASTM D789
Ascend Performance Materials Vydyne® 21Z-NT01A2 Nylon 66, Conditioned
Vydyne® 21Z-NT01A2 is a neat PA66 resin that is designed for extrusion-compounding applications. This grade is unique in its class with its high concentration of amine end groups that is proven to ..