Polymer Property : Relative Viscosity = 4.4 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 4.2 - 4.4 cP
4.2 - 4.4 cP
98% H2SO4
UBE 5033FDX27 Air Blown Nylon 6/66 Film
Specialties: High slip typeMedium shrinkApplications: General purposeSuitable for Water cooling processProcessing: Sausage casings (Water)Big bag (Air blown)Information provided by UBE.