Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 34 - 37 cP | 34 - 37 cP | ASTM D1925 |
Ascend Performance Materials Vydyne® 21ZLV Nylon 66, General Purpose Vydyne® 21ZLV is a lower-viscosity, general-purpose PA66 resin. It is available in natural and designed for extrusion-compounding applications. Vydyne 21ZLV is the feedstock of choice for highly fi.. |