Polymer Property : Relative Viscosity = 3.49 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 3.49 - 3.63 cP
3.49 - 3.63 cP
98% H2SO4
UBE 1022FDX23 Nylon 6 Homopolymer Film
Specialties: High slip typeProcessing: Water cooling processTypical applications: small pouch & generalInformation provided by UBE.