Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 3.31 - 3.43 cP | 3.31 - 3.43 cP | 96% H2SO4 |
UBE 1022FDX29 Nylon 6 Homopolymer Film Specialties: Nucleated (Medium viscosity) Processing: T-die, Air blown Applications: General applications Information provided by UBE. |