Polymer Property : Relative Viscosity = 3.25 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 3.25 - 3.35 cP
3.25 - 3.35 cP
1% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ E 33 L Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™
Relative Viscosity 3.25 - 3.35 cP
3.25 - 3.35 cP
1% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ E 33 LN Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™
Relative Viscosity 3.25 - 3.35 cP
3.25 - 3.35 cP
1% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ E 36 L Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™
Relative Viscosity 3.25 - 3.35 cP
3.25 - 3.35 cP
1% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ 33 Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™