Polymer Property : Relative Viscosity = 3.1 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 3.1 cP
3.1 cP
Correlation, Cyclohexanone 1%; Internal Method
PolyOne Geon™ Specialty Suspension Atlas S140 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Atlas S140 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for intsan..