Polymer Property : Relative Viscosity = 20 cP
Polymer Property :
Relative Viscosity =
20 cP
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Relative Viscosity
20
-
30
cP
20
-
30
cP
Esstech X-166-0151 Poly Methyl Methacrylate/Methacrylic Acid
CAS # 25086-15-1Information provided by ESSTECH, Inc.